What causes concrete spalling, and how urgent is it?
Spalling is usually caused by water reaching the reinforcement, which rusts, expands and cracks the concrete cover. The damage tends to spread and falling concrete is a safety risk, so it should be dealt with promptly. A proper repair breaks out loose concrete, treats the corroded steel and rebuilds the section with repair mortar in layers, while also stopping the water source; otherwise the spalling is likely to return.
Common signs
- Cracked, bulging or spalling concrete on ceilings or walls
- Exposed reinforcement or rust stains
- Cracks under canopies or balconies
- A Buildings Department repair order, or a mandatory building inspection report requiring repairs
Method statement
- Survey and mark-upTap-test to find hollow areas, photograph and mark the repair zones, and set up safety barriers.
- Break out loose concreteBreak back to sound concrete, leaving enough clearance behind the bars.
- Remove rust from rebarClean corrosion from the bars; where section loss is severe, add reinforcement as instructed by the professional.
- Rust protectionPrime the reinforcement with anti-corrosion primer.
- Bonding agentImprove the bond between old and new concrete.
- Repair mortar in layersRebuild the section to its original profile with repair mortar.
- Render and protectionRestore a flat surface and apply a protective coating or paint as needed.
- Photo record and documentsPhotograph every key stage; for works under the Minor Works Control System, submit the required documents.
Systems and materials
| System | Typical use |
|---|---|
| Polymer-modified repair mortar | General spalling repair |
| Rebar anti-corrosion primer | Exposed reinforcement |
| Bonding agent | Interface between old and new concrete |
| Protective surface coating | External walls, canopies and other exposed areas |
We commonly use Nippon and Sika products. The final materials depend on location and scope, and are stated in the quotation.
Testing and records
- Photo record of each stage (break-out, de-rusting, priming, repair)
- Completion inspection
- Statutory documents where applicable
- Warranty typically 1 year, stated in the quotation according to system and scope
Information we need for a quote
- Address and building age
- Photos of the spalling (overall and close-up)
- Estimated area
- Whether a Buildings Department order or inspection report has been issued
FAQ
Can spalling just be plastered over?
No. If the corroded steel is not treated, it keeps rusting and expanding, and the patch will crack again soon.
What should I do after receiving a Buildings Department repair order?
Appoint qualified persons and a contractor to investigate and carry out the repairs within the deadline in the order. As a Class I Registered Minor Works Contractor, we can work with the relevant professionals to carry out the repairs and submit the required documents.
How long does concrete repair take?
It depends on the area, location and access. Repair mortar must also be applied in layers and cured as the manufacturer requires. The programme is stated in the quotation.
Must the water source be fixed at the same time?
If water caused the spalling, the source (for example the roof membrane or a wall crack) must also be treated, or the repair will not last.
How long is the warranty for concrete repair?